WIPIVERSE All articles

Rule based analysis of extrusion process

Rule-based analysis of extrusion process is an approach used to determine a set of design rules essential for consideration while designing an extruded product, or even during the cost estimation of such a product. It applies to extrusion, a plastic deformation process in which a raw material (billet) is forced to flow by compression through a die opening of smaller cross-sectional area. The extrusion process is divided into two basic types: direct extrusion, in which the billet is pushed through the die with ram pressure, and indirect extrusion, in which a die moves relative to the container.

The rule-based analysis covers several categories of design considerations.

Material

The material of the profile to be extruded plays an essential role in determining process parameters and potential limitations. For example, the minimum thickness of extruded carbon steel sheet is 3 mm, whereas the same sheet of aluminium can be extruded into minimum sheet thicknesses of 1 mm. A variety of materials, including carbon steel, aluminium, titanium, magnesium, ABS, and PVC, can be manufactured via extrusion processes.

Profile shape

Extrusion processes can produce a wide variety of profile shapes, but profile features must be considered to ensure product feasibility and strength.

Wall thickness: Strength and cost efficiency are the two main factors when deciding wall thickness. Uniform wall thicknesses are the easiest to manufacture, though thickness can be varied within a profile. Where changes are unavoidable, they should be gradual rather than abrupt. Thick sections adjacent to thin sections should be avoided, as material tends to flow faster where thicker sections occur, giving rise to more expected distortion. For an extrusion process, wall thickness may vary from 1 mm (aluminium) to 32 mm (PVC).

Corner radii: Extrusion processes cannot achieve sharp corners without additional fabrication. Internal corners should be filleted with a minimum radius of 0.5–1 mm, and sharp external edges should be rounded, as those tips can easily become wavy and uneven.

Solid profiles: Solid profiles can reduce die costs and are often easier to produce.

Fewer cavities in hollow profiles: Hollow profiles are often difficult to produce, but a hollow profile can be replaced by two telescoping profiles to ease manufacturing. Reducing the number of cavities in a hollow profile makes it easier to extrude and can also increase die stability.

Profiles with deep channels: For profiles with pockets or channels, a basic rule is that the width-to-height ratio should be approximately 1:3 to ensure the strength of the die is not jeopardized. When using larger radii at the opening of the channel and a full radius at the bottom, width-to-height ratios could rise to 1:4.

Heat sinks: Cooling fins on profiles greatly increase areas for heat dissipation. Surface area can be further increased by giving fins a wavy surface, as an undulating surface increases the heat dissipation area. However, where forced air-cooling is applied longitudinally along the profile, it can be better to leave fins smooth to avoid eddy formation.

Surface finish

The surface finish of exposed product surfaces is an essential consideration during an extrusion process. As a general rule, the narrower an exposed surface, the more uniform its finish becomes. Webs, flanges, and abrupt changes in metal thickness may show up as marks on the opposite surface of an extrusion, particularly on thin sections. Such marking can be minimized with design changes such as rounding transitions, which reduce the chance of opposite-side streaking.

Symmetry

Symmetry provides more balanced forces and helps avoid overstressing areas of the extruding die. Hollow areas within the cross section, in particular, should be balanced.

Length tolerances

Waste tolerances are often included in a required extrusion's length. It can be difficult and expensive to cut a perfect length during production, because metals or thermoplastics expand and contract at different temperatures. Greater accuracy is often possible if lengths are cut off-line. A typical length tolerance for uPVC might be ±1 mm (0.2%) on a 500 mm total length.

Extrusion ratio

The extrusion reduction ratio is the ratio of the cross-sectional area of the shape of the die opening to that of the container through which the billet is pushed. A large-diameter billet pushed through a very small die opening has a high reduction ratio and may sometimes not be possible to extrude. Ratios of 75:1 are common, though difficult. For a difficult ratio shape, one solution is to make the part on a press with a smaller container; another option is to use a multihole die that lets a number of profiles extrude simultaneously, which is also useful for small shapes that are too long to handle practically.

Browse

More topics to explore

    Browse all articles